Tin Lead Sn/Pb Solder Bar i alakaʻi ʻia a me ke alakaʻi ʻole
Hōʻike huahana
Hana ʻia ʻo Solder Bar mai ka metala maʻemaʻe kiʻekiʻe, e hoʻohua i ka lepo haʻahaʻa a me ka hoʻoheheʻe keleawe. He kūpono ia no ka luʻu ʻana, koho a me ka nalu ʻana. No ka hoʻokō ʻana i ka maikaʻi kiʻekiʻe i manaʻo ʻia e hoʻohana wale mākou i ka tin me kahi maʻemaʻe maʻemaʻe o 99.9%. Hiki i ka QLG Solder bar ke hāʻawi i ka hana kūʻai paʻa a me ka wai maikaʻi loa. Ua hana ʻia kēia mau mea kūʻai aku e kūlike i nā kūlana honua a i ʻole nā mea kūikawā.
Hāʻawi kā mākou hui i ke ʻano Tin-Lead a me ke ʻano Lead-Free i hoʻohana ʻia i nā mea like ʻole e like me ke kumu a hoʻopiha i nā mea kūʻai aku no ka nalu, dip a me ke koho koho i ka hana uila.
ʻO ke kaumaha maʻamau 500g a me 1000g, hiki ke hoʻololi ʻia, pono ka MOQ.
Ua lawe ʻia aku kā mākou mea kūʻai aku i ʻAmelika, Jordan, Indonesia, Philippines, India, Pakistan a me nā ʻāina ʻē aʻe. Eia kekahi, ke ʻimi nei mākou i nā ʻelele a me ka mea hoʻolaha a puni ka honua, a hiki ke hāʻawi i ka lawelawe OEM & ODM. Kūkākūkā ʻia ke kumukūʻai kikoʻī.
Nā hiʻohiʻona
1.Excellent soldering hana
2.Ultra High Electrical Conductivity
3.Appropriate activated rosin flux hiki ke hāʻawi maikaʻi i ka hopena fluxing.
4.Fast soldering wikiwiki, a me ka maikaʻi loa fluidness.
5.High anti-oxide
Hāʻawi huahana
● ʻAi-oxide Bar
● Pākuʻi kālā i hoʻohui ʻia
● Paʻa Kino Maʻemaʻe
● Lead Free Solder Bar
Alloy | Maikaʻi alakaʻi | Kaumaha Kūikawā g/cm3 | Lae Metling ℃ |
Sn63Pb37 | Alakaʻi | 8.4 | 183 |
Sn60Pb40 | Alakaʻi | 8.5 | 183-190 |
Sn55Pb45 | Alakaʻi | 8.7 | 183-203 |
Sn50Pb50 | Alakaʻi | 8.9 | 183-215 |
Sn45Pb55 | Alakaʻi | 9.1 | 183-221 |
Sn40Pb60 | Alakaʻi | 9.3 | 185-235 |
Sn35Pb75 | Alakaʻi | 9.5 | 185-245 |
Sn30Pb70 | Alakaʻi | 9.7 | 185-255 |
Sn25Pb75 | Alakaʻi | 9.9 | 185-267 |
Sn20Pb80 | Alakaʻi | 10.2 | 185-279 |
Sn0.7Cu | Ke alakaʻi ʻole | 7.4 | 227 |
Sn100 | Ke alakaʻi ʻole | 7.28 | 232 |
Sn0.3Ag0.7Cu | Ke alakaʻi ʻole | 7.4 | 217-227 |
Sn1Ag0.5Cu | Ke alakaʻi ʻole | 7.4 | 217-227 |
Sn3.0Ag0.5Cu | Ke alakaʻi ʻole | 7.4 | 217-220 |
Hiki ke hoʻopilikinoʻia nā mea hana kūikawā |
FAQ
1. He aha kāu mau kumukūʻai?
Hiki ke hoʻololi i kā mākou mau kumukūʻai ma muli o nā kumu mākeke a me LME. E hoʻouna mākou iā ʻoe i kahi papa inoa kūʻai hou ma hope o ka hoʻopili ʻana o kāu hui iā mākou no ka ʻike hou aku.
2.He aha ke kumukūʻai a me nā hua'ōlelo uku?
ʻO nā hua'ōlelo kumukūʻai e pili ana iā EXW, FOB, C&F a me CIF; ʻO nā hua'ōlelo uku hiki ke T / T.
3.He aha ka palena liʻiliʻi o nā huahana solder?
ʻO ka MOQ o ka uwea solder he 40kg. ʻO ka MOQ o ka pahu solder he 20kg. ʻO ka MOQ o ka solder paste he 20kg.